| Original document(17 pages) 中文版 |
A toner having an amorphous resin, a crystalline resin, and a colorant, wherein the crystalline resin has a melting temperature of at least 70 DEG C and a recrystallization point of at least 47 DEG C exhibits improved document offset properties and improved heat cohesion. Annealing the toner further improves the heat cohesion and morplzology of the toner. |
Application Number 申请号 |
200610067368 |
Application Date 申请日 |
2006.03.24 |
| Title 名称 |
Ultra low melt toners comprised of crystalline resins
|
Publication Number 公开号 |
1837967 |
Publication Date 公开日 |
2006.09.27 |
| Approval Pub. Date |
|
Granted Pub. Date |
|
| International Classification 分类号 |
G03G9/08,G03G15/00 |
Applicant(s) Name 申请人 |
Xerox Corp. |
| Address 地址 |
|
| Inventor(s) Name 发明人 |
Sacripante Guerino G., Zhou Ke, Hawkins Michael S., Nosella Kimberley D., Zwartz Edward G., Mihai Nicoleta, Farrugia Valerie M., Drappel Stephan V. |
| Attorney & Agent 代理人 |
guo anxun li liantao |
|
|