Original document(5 pages)  中文版
    A process for crystallizing aluminum fluoride from the resultant aluminum fluoride solution includes such steps as crystallizing at 130-200 deg.C under 3-5 atom, filtering, washing, and drying. It has high volume weight.
Application Number
申请号
200510017402 Application Date
申请日
2005.03.07
Title 名称 Crystallization method of aluminium fluoride
Publication Number
公开号
1830793 Publication Date
公开日
2006.09.13
Approval Pub. Date Granted Pub. Date
International Classification 分类号 C01F7/50
Applicant(s) Name
申请人
Duo-fluoride Chenicals Co., Ltd.
Address 地址 454191
Inventor(s) Name 发明人 Li Shijiang, Hou Hongjun, Yang Chunhua, Huangpu Genli, Yan Chunsheng, Zhang Liang
Attorney & Agent 代理人 chen gao

  
Method for producing aluminium fluoride
Method for producing cryolite
Spun casting method for cast-aluminium rotor of large-size electric motor
Washing and sizing technology for dress leather
Production of high molecular-ration cryolite by sodium-fluorosilicate sodium-aluminate method
Production of cryolite by hydrofluoric acid and sodium aluminate process
Method for simultaneously producing sodium aluminofluoride and silica white
Method for linked producing ammonium fluoride and white carbon black
Method for linked producing ammonium acid fluoride and white carbon black
Method for linked producing potassium fluoride white carbon black
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.