    A process for preparing the CuCe/FeCrAl catalyst includes such steps as washing FeCrAl carrier with acetone, oxidizing, immersing it in gamma-Al2O3 sol, drying, calcining, quickly putting it in the colloidal solution prepared from copper nitrate, cerium nitrate and citric acid, and calcining.
Application Number
申请号
200610013469 Application Date
申请日
2006.04.18
Title 名称 Preparation method of coppor cerium catalyst coated on FeCrAl carrior
Publication Number
公开号
1830566 Publication Date
公开日
2006.09.13
Approval Pub. Date Granted Pub. Date
International Classification 分类号 B01J37/02,B01J23/83,B01J32/00
Applicant(s) Name
申请人
Tianjin Univ.
Address 地址 300072
Inventor(s) Name 发明人 Zeng Shanghong, Liu Yuan
Attorney & Agent 代理人 li feng

  
Method for preceding to oxidize CO in hydrogen-riched air
Preparation method of light colour high purity sodium polystyrene sulfonate cation exchange resin
Disintegrator and its disintegrating method
Breaking dovice of multi-hammer head breaker
Medium mixing up of wet-type dispersion machine
Vertical ultrafine disintegrator
Separation device used for grain washing
Air purification device
Separation method of bauxite aluminium-silicon miterals
Filtration assembly with open-ended canister
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.