    A heat treating method for preparing the glass able to emit strong blue influorescence from its surface includes such steps as polishing both surfaces of quartz glass, sufficient contact between the polished quartz glass and the mixture of ZnO powder and MnO powder, heating the quartz glass whose surfaces carry said powders to 1000-1200 deg.C, holding the temp for 1-3 hr, and polishing.
Application Number
申请号
200510110417 Application Date
申请日
2005.11.16
Title 名称 Process for preparing glass of lightening strong blue fluorescence on surface
Publication Number
公开号
1792932 Publication Date
公开日
2006.06.28
Approval Pub. Date Granted Pub. Date
International Classification 分类号 C03C21/00,C03C17/23,C03C4/12
Applicant(s) Name
申请人
Huadong Normal Univ.
Address 地址 200062
Inventor(s) Name 发明人 Shi Wangzhou, Sun Linlin
Attorney & Agent 代理人 cheng zongde

  
Preparation method of composite film capable of reducing exciting voltage of quantum spots
Treatment method for optical fiber
Process for protecting film of off-line temperable low radiation film coated glass
Radiation-curable composition and products coated therewith
Composite active carbon fibre and preparation process thereof
Automatic bonding machine for MEMS high temp. pressure sensor
Process for super low temp, anode bonding of microcrystal glass and stainless steel and apparatus thereof
Muitilayer safety tempering glass and production process thereof
Process for prepering active magnesium oxide
Water hardened aluminium oxide pouring material binding agent and preparation process thereof
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.