nature : some non-ferrous metals and alloys, in duplicate or alternating stress, no apparent fatigue limit. Therefore, often required lesser alternating cycles must stress N weeks after the fracture can bear the greatest stress, fatigue called to sign σ N said. N material fatigue life, the general provisions (1 ~ 10) × 107 scope.