Molecular formula : MW : CAS :
nature : a dry method. To the aquifer material shaped into a foam, or without foam, to which blowing gas and rapid mixing, made apparent density is about 0.3 ~ 0.6 bubble stability, and then the bubble in porous materials coated board to a thickness of 5 mm 2 porous foam layer, further ventilation drying. Thermosensitive apply to materials, such as food and medicine, in five to 15 minutes within porous dry products.