Molecular formula : MW : CAS :
nature : refers to the 100 ° C above can still retain their original characteristics and the value of its rubber products and its tributaries. Natural rubber scope of the heat is 100 ~ 125 ° C and 140 ° C SBR about chloroprene rubber around 160 ° C, 175 ° C NBR about acrylate rubber around 200 ° C, silicon rubber and rubber fluoride 200 ~ 300 ° C. In addition to the appropriate use of rubber species, but also with rational use of agents. Commonly used to the heat and heat transfer agent with asbestos powder, mica powder, graphite, silica, clay, zinc oxide, magnesium carbonate, etc.. In exceptional circumstances, it can be aluminum or white lead.